CeramTec Sonox P504
Basic Information
Density:
ρ :
7.65
g/cm3
Curie temperature:
TC:
350
°C
Material class:
Lead Zirconate Titanate
Reviewed:
Yes
Dielectric constant:
-0.40
Coupling constant:
0.10
Resonant frequency:
0.40
Electric Properties
d15:
530.0
*10-12 C/N
d31:
-157.0
*10-12 C/N
d33:
390.0
*10-12 C/N
g33:
25.5
*10-3 Vm/N
tan δ:
0.012
kt:
0.51
kp:
0.59
k15:
0.66
k31:
0.32
k33:
0.71
Elastic Properties
S11E:
16
*10-12 m2/N
S33E:
18
*10-12 m2/N
Qm:
90
N1:
1320
Hzm
N3:
1250
Hzm
NP:
2020
Hzm
NT:
2035
Hzm
Availability
Ceram Tec Gmbh
www.ceramtec.com