MorganTech PZT703



  Basic Information


Density:

ρ :
7.80
g/cm3


Curie temperature:

TC:
270
°C


Material class:

Lead Zirconate Titanate

Reviewed:

No


λ:
1.2
Wm-1K-1


Dielectric constant:
-0.50

Coupling constant:
-0.50

Resonant frequency:
0.50



   Electric Properties



d15:
500.0
*10-12 C/N

d31:
-150.0
*10-12 C/N

d33:
340.0
*10-12 C/N



g15:
33.0
*10-3 Vm/N

g31:
-10.0
*10-3 Vm/N

g33:
30.0
*10-3 Vm/N




tan δ:
0.029


ε33T:
1100



kp:
0.63

k15:
0.68

k31:
0.37

k33:
0.73



   Elastic Properties



S11E:
15
*10-12 m2/N

S55E:
38
*10-12 m2/N



Qm:
80



ν:
0.30



N1:
1500
Hzm

NP:
2100
Hzm



Availability


Morgan Technical Ceramics
http://www.morgantechnicalceramics.com/